Fabrication of vertical flanks with CAR 44
AR-N 4400-50 was investigated at the TU Braunschweig with particular regard to the fabrication of well-defined resist architectures with vertical flanks.
AR-N 4400-50 was investigated at the TU Braunschweig with particular regard to the fabrication of well-defined resist architectures with vertical flanks.