Innovative new development at the MNE 2017
Allresist participated in the conference as a “silver sponsor” with an own large stand and presented many remarkable new developments. A particular highlight was our scientific poster on our new development AR-N 4600 (now Atlas 46) and the lecture by Dr. Gerngroß about this interesting negative photoresist.