HSQ E-Beam Resist AR-N 8400 series (Medusa 84 SiH)

(AR-N 8400.04, AR-N 8400.08, AR-N 8400.12, AR-N 8400.22)

High Resolution. Improved Stability. MIBK-Free.

Combining outstanding nanoscale resolution with enhanced storage and process stability, Medusa 84 SiH offers a powerful alternative to conventional MIBK-based HSQ formulations.

Its innovative butyl acetate-based formulation eliminates MIBK as a solvent while maintaining the excellent lithographic performance expected from HSQ resists.

Discover a More Stable HSQ Resist

Looking for a reliable alternative to conventional HSQ resists? Our technical team will help you evaluate Medusa 84 SiH for your lithography process.

Request a evaluation sample or contact our experts for technical advice.

Characterisation

Outstanding Nanoscale Resolution
  • Highest resolution of 3.5 nm lines
  • Excellent plasma etch resistance
MIBK-Free Formulation
  • Hydrogen silsesquioxane dissolved in butyl acetate
  • No MIBK used as formulation solvent
Enhanced Shelf Life and Process Stability
  • Stabilized formulations for improved storage and processing reliability
  • Guaranteed shelf life of 6 months for ready-to-use resist solutions under recommended storage conditions
  • Potential for extended shelf life through deep-freeze storage
Ready-to-Use HSQ Solutions
  • Pre-formulated liquid resists
  • Multiple concentrations for different film thickness requirements
  • No powder dissolution required
Designed for Advanced Nanofabrication
  • High-resolution electron beam lithography
  • Nanoscale patterning
  • Semiconductor research
  • Photonic and optical nanostructures
  • High-resolution etch masks
  • Advanced micro- and nanotechnology research

Important user information

Medusa 84 SiH must not be transferred to glass containers or filtered using a glass pre-fi lter, as this will cause it to gel irreversibly.
The Medusa 84 SiH has to reach room temperature before opening the bottle. Condensing water can affect the shelf life, as the resist is sensitive to moisture.

New Product Development

Our compatible choline-based developer AR 300-41 (TMAH-free)

Properties

  • Film thickness/4000 rpm:  50 nm
  • Flash point (°C):                  <35 °C
  • Storage 6 month:              8-12 °C

Available order sizes

  • 1x 30 ml (experimental sample)
  • 1 x 100 ml
  • 1 x 250 ml
  • 1 x 1000 ml

Please contact us for further requests.

Structure resolution

Single lines with a resolution of 3.6 nm and very low LER written with the RAITH Voyager EBL-System at 50kV, 120 pA, dose: 14.700 pC/cm, developer: KOH 1% 1 min. © Raith Dortmund

Resist structures

100 nm line/space structures written on silicon at 1000 μC/cm² @ 100 kV and developed with AR 300-73 (6.5% TMAH solution). © J. Hohmann, KIT-IMT Karlsruhe

Structures with a high aspect ratio

Left: Wall-structures written on GaAs with 600 μC/cm² @100 kV, 200 pA, developed with AR 300-73 (6.5% TMAH) for 60 s, PAB & PEB: 5 min @ 100 °C hotplate. © Yurii Kutovyi, FZ Jülich

Right: Nanorod written on silicon with 2000 μC/cm² @ 50kV and developed with AR 300-44 (2.38% TMAH). Aspect ratio of up to 10 was achieved. © R. Stöhr, ZAQuant University of Stuttgart

Medusa 82/ 82 PAG and new Medusa 84 SiH from 2025 onwards

In a subsequent R&D phase, Allresist enhanced the resolution and plasma etching resistance by optimising the synthesis of the HSQ polymer. The new chemical composition of Medusa 84 SiH exactly matches that of HSQ (hydroxysilsesquioxane). Furthermore, stabilisers now extend the shelf life of Medusa 84 SiH. Our new Medusa 84 SiH achieves resolutions of < 10 nm with higher plasma etching resistance and an improved adhesion compared to Medusa 82/82 PAG. Process and storage stability for low solid content variants such as SX AR-N 8400.04 (50 nm @ 4000 rpm) and SX AR-N 8400.08 (100 nm @ 4000 rpm) is guaranteed for 6 months when stored in a refrigerator (10 °C). Deep-freeze storage extends the shelf life further.

Read more about this in our customer letter.

    Product Request

    *Name

    *Company/Institute

    *E-Mail

    *Subject

    *Your Message