Protective coating to prevent mechanical damage

Sensitive substrates can be protected against damage during handling with resist SX AR-PC 5000/3.1, which is especially important in the case of double-sided procedures. This novolac-based resist is applied by spin coating and tempered. After handling, the resist can easily be removed with conventional removers.