Thinner X AR 300-74/1

For adjusting the coating thickness of the SX AR-PC 5000/41 protective coating

Characterisation

  • ultra-filtered, organic solvent mixture of high purity
  • Coating thickness adjustment of SX AR-PC 5000/41 through defined dilution
  • Edge stripping of coated substrates and device cleaning

Interesting Resist Wiki articles

Properties

  • Main component
    Ethylbenzene
  • Flash point (°C)
    15°C
  • Water content max.
    0,1%
  • Filtration (μm)
    0,2
  • Non-volatiles max. (%)
    20 ppm

Available order sizes

  • 1 x 1.000 ml

Please contact us for further requests