Resist für die Startseite (Resist des Monats)

January 2023: Standard resist AR-P 3510 – 30 years on the world market

Right from the beginning, the idea of sustainability was firmly anchored in the philosophy of our young company. One of the first advanced developments of Allresist was the replacement of teratogenic solvents in the positive photoresist AR-P 351 with safer solvents. This is how the standard resist AR-P 3510 was created, in which the excellent lithographic properties of AR-P 351 were retained, but the resist was now significantly less dangerous to health for the user.

October 2022: Optimised Electra 92 – a new AR-PC 5092

We have now achieved a quality of aniline polymers that does not require the addition of isopropanol, which also increases the stability of AR-PC 5092 resist mixtures. Long-term tests demonstrated that the storage stability is significantly higher than with previous Electra variants.

July 2022: Our resist triplet of the month – presented at the Triple-Beam (EIPBN 2022)

After the corona-related merely online possible presence in the past two years, Allresist finally again took part live at the EIPBN in New Orleans, and we experienced a high interest in our resists at our booth.

April 2022: New environmentally friendly developer for PMMA resists AR 600-57

Exceptionally we present a new PMMA developer in the “Resist of the month” section today, because its potential possibilities will probably also inspire our users. This developer is a mixture of isopropanol and water – which may sound surprising at first, since both components individually do not attack PMMA layers.

January 2022: Versatile Phoenix 81 (AR-P 8100)

Phoenix 81 was developed as part of a Eurostar project in cooperation with Swisslitho AG (now Heidelberg Instruments Nano). Using a NanoFrazor and thermal scanning probe lithography (t-SPL), structures as small as 10 nm can be written by dipping a hot needle into the resist layer and evaporating the resist at the tip (see also AR NEWS, 42nd issue).

October 2021: More efficient production of Electra 92

Many companies meanwhile use the conductivity of Electra layers for their processes and technologies. Since its introduction on the market in 2018, synthesis and processing of Electra have continuously been improved. The conductivity of this resist could for example be increased by a factor of five between 2018 and 2020.

July 2021: CAR 44 for galvanic molding

The successful evaluation of our development at one of our largest customers was the reason for us to select AR-N 4400-50 as resist of the month of July.

April 2021: CSAR 62 – In demand around the world

Resist CSAR 62 is meanwhile established worldwide, with continuously increasing demands. Since we manufacture the polymer by ourselves, we had to scale up polymer synthesis. First of all, CSAR 62 made the jump from laboratory scale to a 20-liter trailer.

January 2021: Optimised process for negative photoresist Atlas 46

We continued the development work on our new Atlas 46 photoresist also in 2021. Due to own results or recommendations and requests from our users, its formulation and properties were now improved.

July 2020: Bottom resist AR-BR 5400, the “workhorse” for two-layer processes